Re: Welding Crankcases

Initially it struck me that it could be "hot shortness" - a phenomenon that affects welded aluminium and creates never ending cracks in the cooling weld pool. Usually recified, if my memory serves me right, by a change in the filler rod composition. The welding supplies people should be able to help with a better filler (probably with more silicon).
It's over 20 years since I studied the welding of aluminium alloys for my thesis so my memory is being hard worked on this one!

The other option might be thermal cracking - but the 200C preheat suggests that isn't the issue.


Charles

Email  
Re: Re: Welding Crankcases - by David Howe - Jan 30, 2007 9:07pm
Re: Re: Re: Welding Crankcases - by Bill Sheehan - Jan 30, 2007 9:42pm
Re: Re: Re: Re: Welding Crankcases - by Bill Sheehan - Jan 31, 2007 3:02am
Re: Welding Crankcases - by Doug Baker - Feb 2, 2007 7:15am