I have read the correspondence with interest, wanting to learn by others experience and in the knowledge that I have to deal with a nasty case of micro blisters on my RP.
I was introduced to a product "Fertan Rust Converter" in 1985. I had just bought a new Renault 4 van and made a 2" scratch on the nearside with the handle of a wheelbarrow, right through to the metal. Rather cross with myself and fearing that the red lace would soon follow I was reassured that an application of Fertan would do the trick. I borrowed some and painted on one application to wet steel.
I never got around to painting over the scratch and in 2001, the van was scrapped after being punted up the back (inevitably by a young driver with no insurance) It sat on my drive for two years while I mourned its passing and was finally towed to the scrap man. The 2" black scar was still there and had not spread at all. the edges being firmly attached paint.
I have recently moved my workshop and retrieved a steel workbench that had sat under tarps in the garden for two and half years. It had a lot of surface rust on the bare top and the legs were quite scabby where they had been exposed. An hour with a wire brush in an angle grinder and a coat of Fertan has transformed it into a rust free black steel bench. I shall get around to painting it later (well maybe). There is no rust after six weeks and it smells great.