Re: Re: Dreaded Marzak Malady

Any attempt to repair this stuff that involves heat is likely to end in tears. These carbs are made of an alloy of uncertain (and possibly variable) composition, consisting mainly of zinc (90% plus). It is the impurities in the zinc that cause them to crumble, a phenomenon known by the expressive German term "Zinkpest".

Now, the melting point of the alloy is around 430C. "Alutight" melts at 380C: fine for aluminium alloys which melt at 600C plus, but you're really staring into the abyss if you try to to repair a precious carb with this product or with Lumiweld which melts at a similar temperature. There are ways of reducing the risk, but for ordinary mortals adhesives are really the only way to go.

Finally, it is probably incorrect to refer to these carbs as "Mazak", since this trade name was not introduced until the 30s, to describe an alloy made using a very pure form of zinc (known everywhere outside the UK as "Zamak" (standing for zinc, aluminium, magnesium, copper). Because of the purity of the zinc, articles made of Mazak/Zamak do not disintegrate (although they may snap like twigs - think of 1960s car door handles, etc.)

I've tried to keep it simple, but if it crumbles it's not (strictly speaking) Mazak!

Email  