I agree Tony, it is very unfair to expect an infinite life from any original crank thrashed. Unfortunately many have a wierd grasp of reality. Possibly 60 to 90% of the total life in normal use is consumed before the first crack appears. Life if thrashed from new would be a fraction of the normal anyway.
Thrashing includes high cr. Peak pressures increase in proportion to the cr!
The Phoenix cranks are apparently nitrided. I am not sure that many are aware of the potentially huge beneficial effect of nitriding on fatigue life. It produces an almost everlasting hard bearing surface but with white metal this is not a serious problem with the standard cranks(filter or not!). The great improvement in fatigue induced by nitriding is presumably the factor which renders the Phoenix cranks so satisfactory.
In fatigue tests nitriding often raises the fatigue limit 20% or more. This means a 20% increase in stress for the same life, but a vastly greater increase in life at the same stress ie commonly 100% to several hundred %.
Problems with nitriding arise in the rare situations when regrinding is required. Heat cracks are easily created. And it is an expensive process to repeat.