I think the problem with zinc die cast carburettors, fuel pumps, door handles, PA speedos etc is the same as that which affects some pre war Dinky toys. I quote from Hornby Dublo 1938-1964 by Michael Foster these models are made from Mazac 5 comprising 4% Aluminium, 0.04% Magnesium, 1.0% Copper and 94.86% Zinc and the Zinc must have a purity level of 99.9%. The accidental intrusion of just 0.1% lead in the metal mix is sufficient to produce a a cracked or powdery casting in due course of time. The problem was most severe in the late 1930s with reports of the workmen saying that on occasions the wire binding the sack of zinc portions was thrown into the melting pot whilst on another occasion the silver paper from a cigarette packet went in. It was reported that when Meccano opened their disply of prewar models in 1946 some had disintegrated on the shelves. The changeover to war material production and the high quality control neccesary improved the situation and modern zinc die castings do not suffer the same problem.
So remember this the next time you think about buying a 22FZB at an autojumble-look for any signs of powdering of the casting.
Happy autojumbling, Dave
I see you have an editing programme which deletes the old slang 3 letter word for cigarette.