The Instruction for an Ammco surfacing hone is to use copious Ammco oil.
The instructions for a Ritch brand rigid hone state to use kero for finishing, followed by oil and 8 parts kero to polish.
Cutting is most rapid with oscillation as reqd for the cross hatch and with copious liquid.
Another source for a rigid hone reommends viscosity of 7.5 mm mm/sec, however that relates.
Ring manufacturers state that the bores should be scrubbed with soap and water until a white rag stays clean
I had a set of Jowett liners rebored by a practioner who claimed to have a suitable jig. The result was .003 out of round. He said he would refund if I could do better. So I spent a few days adjusting my super crudely made Indian lathe and did a set. I got my money back.
Finished with the Ammco hone with oil in kerosene.
If filing nails is too tedious a primitive version of the telescopic gauge is not hard to make. Working to one meaurement standard reduces errors which can quite easily stack up to .001. Hence the value of the feeler test.