Wiping metal is not lead; it is 30% tin or somesuch which gives prolonged pastiness. And is expensive, unless like me your father was a plumber and you have inherited a stash.
Why struggle with panel distortion and sniff acid and lead fumes and absorb lead and contaminate workshop with lead dust and filings? Also risk of explosions due damp containers, burns due solder getting behind rings etc etc. Every trace of rust has to be removed for complete tinning, not just killed.
Cars are going to be molly coddled anyway. The door interiors, window seals, etc are not made for prolonged outdoor life.
The best feature of wiping metal is that it has no shelf life.
If you fancy trying it have go. Struggling with new techniques is all part of the fun. I've never tried lead loading but I've spent endless hours on steaming ash with very mixed results, fascinating and tricky.