The blisters are caused when water vapour penetrates the paint film and set up forces sufficient to weaken the adhesion between the various coats as a result blisters containing water may form. There are other things that can cause blistering, they include 1,Surface contamination. 2,Insufficient undercoat or top coat, 3,Using the wrong thinners, 4,Contaminants in compressed air, 5,Exposing the finish to wet or high humidity before the paint has hardened.
If the blisters are only on the top coat flatten off with abrasive paper until all signs have gone and respray, if the blisters go deeper strip back to bare metal and use a phosphoric acid metal cleaner and conditioner with steel wool.
Make sure all surfaces are clean and free from contamination, change the flatting water frequently and remove all residues, do not touch the surface with bare hands, use a warm workshop and allow the panels to reach the same temperature before spraying, drain the compressor tank of water before spraying and use a water filter in the line, apply the recommended thickness of primer and top coat and allow adequate flash off and drying times between coats and do not allow the paint work to be exposed to wet or humid conditions until it has dried out thoroughly.
Location: Pembrokeshire
Dave Wortley
Feb 5, 2016 - 3:14PM
Re: paint blistering after cold weather
John,
My car is going the same way as yours after it had a couple of winters in a leaky garage. I am trying to ignore it and regard it as that word favoured by the antique world, that is "patina".
Dave.
I'm with you on that. My RP is tidy enough but it's got plenty of "patina" too - I bought a 5 gallon drum of it from Woolworths before they went bust and there's still some left. .
Over restored cars tend to be cossetted and not used much for what they were intended, ie being driven. Not that there's anything wrong with that, just not my thing.
Seeing the other painting thread, is something hand painted with something like tekaloid more or less likely to result in future blistering problems? Obviously, used on clean metal.
Steve Jones
Feb 13, 2016 - 6:10PM
Re: paint blistering after cold weather
Many canal boats are painted with coach paint like Tekaloid or similar as are most steam locomotives!
As you can imagine, it's a lot more than sticking your brush in a tin and slapping the paint on. I'm very happy with my efforts but Malcolm is better than me at coach painting and his efforts are better. All down to experience I think.
In particular, note the tips about not thinning coach paint with turps/white spirit. I've found that conditioners such as Owatrol not only slow down the paint but, according to what is says on the tin, improve the waterproofing properties of the paint. I first painted my Ulster in August 2013. You might recall that the weather then was, what we call in Yorkshire, 'Mad Hot'. I was struggling with the paint going off much too fast because of the high temperatures and looked to find a tin of Owatrol based on the recommendations on the web site. I'd tried White Spirit but that had made things even worse. The local boat chandler explained that it was in short supply because it had all been bought up by people taking advantage of the good weather and painting their boats. They'd one tin left and it sorted the problem.
Maybe this issue is a result of traditional coach paint that was oil based being replaced with coach paint that is acrylic based, perhaps to its detriment.
Anyone having parts soda blasted, please be aware that the process leaves a protective anti-rust coating behind that MUST be thoroughly washed off prior to applying paint.
Geoff - Fixing my lathe, it being far too cold in the Carport.