The lead content was removed from cellulose some years ago and since then it has lost a lot of the qualities it once had.It is and always has been an air drying product and will react if not given enough time to dry between coats.i.e.If the first coat is not allowed to dry any subsequent coats are likely to crack(shear).
I am trying an air drying paint at the moment which it is claimed has more of the qualities of the original stuff ,It's user friendly,durable ,and has a better depth of shine .Whatever, I would always lay it on a good two pack primer/filler.
Dave
That's interesting Dave, do you know when the lead was taken out? Thirty and forty years ago I sprayed a lot of cellulose and had plenty of problems, but never cracks. I often sprayed a panel and then sprayed it again straight away with no drying time at all.