The term glazed is much used. To those as myself whose experience is limited mainly to their few own cars it is something of a mystery. A polished bore can be a sign of wear, but also is often associated no ongoing wear! After the hone marks have gone just what does a healthy high mileage bore look like? My low geared everyday 1960s car at 170,000 miles and just .003 taper, and burning little oil, was not matt.
Is the term an abbreviation for prematurely glazed?
The topic of running in procedure is inferred again. ACL, who were main suppliers of new and replacement rings in Australasia, for conventional lubrication systems, and primarily plated rings, recommend bringing up to temp at a fast idle, then repeatedly accelerating through lowish to medium rpm at wide throttle, with spells of overrun and light running between.
For plain iron rings they considered honing unnecessary, and with the risk of contamination, even undesirable.
And David, do you mean valve seats are small dia or narrow. In general, the latter is beneficial to breathing.