To get a quick overview of all the messages click on
" Switch to Threaded style "
Forum access seems to be restored after the IP address mysteriously blocked. Computers are indeed mysterious!
So here are some more heretical ideas for open minded thinkers to ponder.
Of all the cracked and broken cranks I have seen on Sevens and another notorious make, all failed from the inside radii. This would suggest that in the Seven situation keeping foot firmly on the clutch pedal would likely prolong life!
It is bad practice to fit constrained deep groove ball races to both ends of any shaft. Without a giant Belleville washer or somesuch it is difficult to clamp the rear bearing without compromising flywheel fit. Possibly if the rear only is constrained the front may hammer the timing gears as the crank shortens and lengthens with the firing pulses.
In the highly revved failed Phoenix cranks illustrated it would be interesting to know where the cracks started. Usually obvious from the tide marks.
Nitriding is presumably the main feature of Phoenix cranks which accounts for superior life. Nitriding reduces the sensitivity to section changes and considerably raises the fatigue stress limit. On the other hand small increases in stress greatly reduce fatigue life and with todays running even the cranks on unmodified cars are subject to more stress than most cars in their day. Raised cr and advanced spark both increase stress markedly.
Anything which damages or cracks the nitride layer, regrinding, grinding cracks due wrong wheel, gross overload due hydraulic lock or suchlike calamity, straightening, dropping on end etc may eliminate the nitride protection.
It is generally reckoned that for low cr engines not prone to torsional oscillations, torque has little influence on crank failure. It is bending which causes trouble. The mystery is that cranks, unlike bridges, so often fail at or near the ends where bending moment is least. I don’t know what the explanation is. Presumably the experts can explain.
My theories would no doubt be rubbished with relish.
I cannot see how state of the bearings in a 2 bearing engine would contribute.
Bob Culver
Location: Auckland
Bob
Have you heard of the floppy flywheel?
I believe it was Rob Beck who posts on here who came up with it.
Essentially it was like a modern dual mass flywheel albeit constructed very much in a 750 mc style!
From my vague recollection of the article there was a reason to do with the flywheel and the harmonic period that broke cranks at the rear main. Maybe someone familiar with the floppy flywheel can comment?
All the best
Steve
Location: South East Cornwall
Hi Steve
Have read about but not all the reasoning for. I dont think harmonics have got much to do with it, but obviously from the common mode of failure the non rigid flywheel centre must assist.
Bob Culver
Location: Auckland
Steve,
Nick's article can be found here: http://a7ca.org/flywheel.php
I notice that Colin was sufficiently bold to ask for an opinion on shot peening!
My father broke a steering arm 60 years ago and it triggered a life long curiosity about metal fatigue. My knowledge may be of interest to others.
Any process which places the surface layer in compression gives a degree of protection against fatigue. It was once the fashion to polish aircraft and other conrods but it eventually dawned that it was the working of the surface metal and not the shine which was beneficial. Shot peening, rolling, have been proven vastly more effective.
Many absorption case hardening processes achieve a compression which is why heavily loaded and aircraft and auto gears resist fatigue. Nitriding is one such process.
(Chrome plating has the opposite effect! Not the way to restore worn journals)
Provided there is no existing crack (other than microscopic), and it is not a nitrided Pheonix crank, shot peening should assist.
The problem is that Seven cranks do not only fail at the last one or two radii!
My experience is limited to just ten or so cranks. I laboriously but at no cost test using a magnet and fluid. If any sign that the bearing journal has been heated I start there. That eliminated all those cranks! Of the rest, cracks were found at the next and/or the next radius forward. Apart from the one in the car, I have yet to test a good one! I don’t look for more once one crack is found!
It is often claimed that if prior to a crack a thin layer is removed, fatigue life more or less starts afresh. On that basis decades ago on my car, following an engine wrecked, and before the advent of cheap rotary grinders, I filed all the inner radii large with a chainsaw file and polished! It would not have improved balance but that has little effect on stresses anyway. Cannot comment on effectiveness as only did 20,000 or so subsequent miles.
The time you locate a candidate, crack test, regrind, shot peen all radii on a stock crank, would be well on the way of cost of a Phoenix.
And then it might fail at an oil drilling!
Modified engines are at greatest risk. Raising cr from 5:1 to 7:1 raises peak firing stresses maybe 40%, a colossal increase when fatigue life is critical.
Bob Culver
Location: Auckland
Location: Oxfordshire
Hi Andrew
It probably is technically superior. But it requires use of a ball race which Austin apparently considered inadequate, at least in 1922, and there is the problem of very postively locating it on both shaft and in housing. As is, the rear bearing just relies on its press fit.
Expansion would have a tiny effect on timing but this is not as super critical as many imagine.
The comment about the shaft possibly pulsating in length, or trying to, as it flexes was not entirely tongue in cheek.
It is considerations of expansion which make it bad practice to constrict a shaft with rigidly located ball races at both ends.
Bob Culver
Location: Auckland